Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 558 MPa | 81000 psi | Typical |
Kinetics MIM F75 (ASTM F75) HIP Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |
|||
Tensile Strength, Yield | 558 - 683 MPa | 81000 - 99000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, Spring Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Yield | 558 - 655 MPa | 81000 - 95000 psi | 0.2% offset |
Eagle Brass 511 Phosphor Bronzes 4%, Extra Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Yield | 558 - 621 MPa | 81000 - 90000 psi | 0.2% offset |
Eagle Brass 715 Copper Nickel 30%, Spring 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |