Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 815 MPa @Strain 0.200 % |
118000 psi @Strain 0.200 % |
|
Haynes 625 alloy, plate after 16000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 815 MPa @Strain 0.200 % |
118000 psi @Strain 0.200 % |
|
Haynes 625 alloy, plate after 4000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |