Mechanical Properties Metric English Comments
Tensile Strength, Yield 819 MPa

@Strain 0.200 %,
Temperature 760 °C
119000 psi

@Strain 0.200 %,
Temperature 1400 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Tensile Strength, Yield 819 MPa

@Treatment Temp. 649 °C,
Time 2.88e+7 sec
119000 psi

@Treatment Temp. 1200 °F,
Time 8000 hour
0.2%. Room temp test after thermal exposure
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened, after long term high temperature exposure
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..