Mechanical Properties Metric English Comments
Tensile Strength, Yield 575 MPa

@Strain 0.200 %
83400 psi

@Strain 0.200 %
Haynes 214® alloy, 10% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Yield 575 MPa

@Strain 0.200 %
83400 psi

@Strain 0.200 %
Haynes 625 alloy, 40% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..