Tensile Strength, Yield 57.6 MPa
8350 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ PPH-20G Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Strength, Yield 57.6 MPa
8350 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ PPH-20G Nat Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Strength, Yield 57.6 MPa
8350 psi
ASTM D638
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
Tensile Strength, Yield 57.6 MPa
8350 psi
ASTM D638M
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure
DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur..