Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 84000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 579 MPa

@Strain 0.200 %
84000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, GTAW, as welded, notched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 579 - 731 MPa
84000 - 106000 psi
0.2% offset
Eagle Brass 64725 MAX251C, Extra Hard
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In..
Tensile Strength, Yield 579 - 689 MPa
84000 - 100000 psi
0.2% offset
Eagle Brass 770 Nickel Silver 18%, 3/4 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Tensile Strength, Yield 579 MPa

@Strain 0.200 %,
Temperature 732 °C
84000 psi

@Strain 0.200 %,
Temperature 1350 °F
Carpenter Thermo-Span® Fe-Co-Ni Superalloy
Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h..
Tensile Strength, Yield 579 MPa

@Strain 0.200 %
84000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, GTAW weld, 316L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Copyright © lookpolymers.com All Rights Reserved