Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 57.93 MPa | 8402 psi | ASTM D638 |
Lucent Polymers 66-41 Nylon 66, Toughened Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |