Polymer Property : Tensile Strength, Yield = 841 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.80 MPa
841 psi
cured 72 hrs @ RT
ACC QM 260 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
QM 260 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th..