Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.196 - 58.8 MPa | 28.4 - 8530 psi | Average value: 3.54 MPa Grade Count:57 |
Overview of materials for Styrene/Butadiene/Styrene (SBS) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o.. |