Mechanical Properties Metric English Comments
Tensile Strength, Yield 593 - 641 MPa
86000 - 93000 psi
0.2% offset
Eagle Brass 260 Cartridge Brass, Extra Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Tensile Strength, Yield 593 MPa

@Strain 0.200 %
86000 psi

@Strain 0.200 %
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 15% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
Tensile Strength, Yield 593 MPa
86000 psi
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 10% Cold Rolled (UNS S30200)
This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to ..
Tensile Strength, Yield 593 MPa

@Strain 0.200 %
86000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), notched