Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 87.9 MPa | 12700 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 1200 A Zip 22 Natural Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |