Polymer Property : Tensile Strength, Yield = 8881 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.23 MPa
8881 psi
ASTM D638
ACC EP QSZ EPI Engineered Polymers Quick Set Epoxy with Zinc
EP QSZ Quick Set Epoxy with Zinc, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s (Volatile Organic Compound), self-leveling modified epoxy. This versatile new gene..
Tensile Strength, Yield 61.23 MPa
8881 psi
ASTM D638
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy
EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast..
Tensile Strength, Yield 61.23 MPa
8881 psi
ASTM D638
ACC EP QS EPI Engineered Polymers Quick Set Epoxy
EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure..