Polymer Property : Tensile Strength, Yield = 8910 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.4 MPa

@Thickness 3.17 mm
8910 psi

@Thickness 0.125 in
KEP Kepital® F20 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 61.4 MPa
8910 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release..
Tensile Strength, Yield 61.4 MPa
8910 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 893-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 893-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release..