Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 897 MPa | 130000 psi | 0.2% Offset |
ATI Allvac® 6-6-2 Titanium Alloy, Heat Treatment: 718°C (1325°F) Anneal Data provided by Allvac.Applications: Airframes, jet engines, rocket engine cases, nuclear reactor components, ordnance components. |
|||
Tensile Strength, Yield | 897 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 9310 Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization Data provided by Allvac.Applications: High performance helicopter transmission gears, components. |
|||
Tensile Strength, Yield | 897 MPa | 130000 psi | EN2597B |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/280H5/AS4-3K Fiber: AS, Weave: 5HS, 280 g/m2Information provided by HexCel |
|||
Tensile Strength, Yield | 897 MPa @Strain 0.200 % |
130000 psi @Strain 0.200 % |
|
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age Data provided by Allvac.Applications: Turbine compressor blades and discs, shafts, spacers, fasteners, miscellaneous jet engine hardware; space shuttle turbo pump seals.Waspaloy is a registered trad.. |