Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.35 MPa
1360 psi
-15% change after 168 hours @ 125°C; ASTM D412
Precision Polymer Engineering E70E Ethylene Propylene Rubber
Ethylene Propylene Terpolymer, 66-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace Specification DTD5597A Grade 70.Applications: For sealing applications where goo..
Tensile Strength, Yield 9.35 MPa
1360 psi
10% change after 168 hours @ 200°C; ASTM D412
Precision Polymer Engineering S80U Silicone Rubber
Translucent Silicone Rubber, 70 -80 °IRHD. Shore A Platinum cured Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Silicone compound in conformity with the req..