Polymer Property : Tensile Strength, Yield = 9.970 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.970 MPa
1446 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer
Elastocon® 8088N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8088N is FDA compliant and well suited..