Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Tensile Strength, Yield | 90.3 MPa @Temperature 22.8 °C |
13100 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger Sintimid™ V 15% graphite Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | oriented film, Yield Stress |
Honeywell Aegis™ CSD High Barrier Nylon
(discontinued **) Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Solvay Technyl® A218 Heat Stabilized Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES Electrablend® PC SS15 FR BK 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 E2 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 E40 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 HS YL030 Heat Stabilized Availability: North AmericaForms: PelletsFeatures: Fast Molding Cycle and Good AdhesionAppearance: YellowTPCI# 10054102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 L LE MB Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Low ExtractablesAppearance: Colors AvailableTPCI# 7964102Information provide.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 L N MB (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 L N YL038MB Availability: North AmericaForms: PelletsAdditive: Lubricant, UV Stabilizer and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Good UV Resistance and NucleatedAppeara.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 L UV (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 LE BK (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Low Extractables and NucleatedAppearance: BlackTPCI# 7.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES HiFill® PA6 X BN071 EL MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Fast Molding Cycle, Good Processability, Lubricated and NucleatedTPCI# 1033102Information provided by TP Co.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 L N BK MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Fast Molding Cycle, Good Processability, Nucleated and LubricatedTPCI# 7970102Information provided by TP Co.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 L N BK002 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and Lubricant(4500 ppm)Features: Fast Molding Cycle, Good Processability, Nucleated and LubricatedAppearance: BlackTPCI# 1327102In.. |
|||
Tensile Strength, Yield | 90.3 MPa | 13100 psi | ASTM D 638 |
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer Description: Hostacom™ PF062-3 high melt flow, 5,200 MPa flexural modulus, chemically coupled, 30% glass fiber-reinforced polypropylene homopolymer has good impact strength, high stiffness and very.. |