Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 62.3 MPa @Thickness 3.20 mm |
9030 psi @Thickness 0.126 in |
10mm/min; ASTM D638 |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |