Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 927 MPa @Strain 0.200 %, Temperature 538 °C |
134000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |