Polymer Property : Tensile Strength, Yield = 9360 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.5 MPa
9360 psi
ASTM D638
Spartech PC-2000 High Impact Polycarbonate Sign Grade Sheet
Description: Sign Grade SheetInformation provided by Spartech.
Tensile Strength, Yield 64.5 MPa
9360 psi
ASTM D638
Spartech Sungard Ultra Weatherable Polycarbonate Sign Grade Sheet
Description: Sign Grade SheetInformation provided by Spartech.
Tensile Strength, Yield 64.5 MPa
9360 psi
ASTM D638
Spartech UltraTuf SG Polycarbonate Sheet
Description: Polycarbonate SheetInformation provided by Spartech.
Tensile Strength, Yield 64.5 MPa
9360 psi
ASTM D638
Spartech UltraTuf SP-7010 Polycarbonate Sheet
Description: Polycarbonate SheetInformation provided by Spartech.