Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 945 MPa | 137000 psi | |
HP Alloys Alloy X, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International. |