Polymer Property : Tensile Strength, Yield = 946.4 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.525 MPa
946.4 psi
-25% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G50S FFKM White Perfluoroelastomer
Perlast® G50S FFKM is a White Perfluoroelastomer 50-55 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and extr..