Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 95.8 MPa | 13900 psi | ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Tensile Strength, Yield | 95.8 MPa | 13900 psi | ASTM D638 |
Teknor Apex Sinpolene GPP1640 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 40% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Tensile Strength, Yield | 95.8 MPa | 13900 psi | ASTM 638 |
PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |