Mechanical Properties Metric English Comments
Tensile Strength, Yield 665 MPa

@Strain 0.200 %,
Temperature 315 °C
96500 psi

@Strain 0.200 %,
Temperature 599 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 665 MPa

@Strain 0.200 %
96500 psi

@Strain 0.200 %
Haynes 625 alloy, plate after 16000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 665 MPa

@Strain 0.200 %
96500 psi

@Strain 0.200 %
Haynes 25 alloy, room temperature after 20% cold reduction, 1065°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..