Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.69 MPa | 970 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 0921 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 6.69 MPa | 970 psi | ASTM D412 |
Teknor Apex Vidux® CV-1000-88 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-AntistaticForms-PelletsProcessing Method- ExtrusionInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.69 MPa | 970 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui.. |