Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 993 MPa @Strain 0.200 % |
144000 psi @Strain 0.200 % |
|
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Rod, 3 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter Tensile strength (ultimate and yield), shear strength, reduction of area, and elongation values reported here are typical for Hot Finished Rod, 3 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter s.. |
|||
Tensile Strength, Yield | 993 MPa @Strain 0.200 % |
144000 psi @Strain 0.200 % |
68°F (hardened to 350 HB) |
Bohler-Uddeholm BÖHLER RAMAX® HH Modified 420F Chromium alloyed steelTypical applications for Ramax® HH are: holders and bolsters for plastic molds, plastic and rubber molds with low requirements on polishability, and dies for plastic extrusion.. |