Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 220 g @Thickness 0.0200 mm |
0.485 lb @Thickness 0.000787 in |
ISO 7765-1 |
Total MDPE HF 513 Medium Density Polyethylene, Blown Film MDPE HF 513 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HF 513 is a semi-high molecular weight polyethylene giving excellent mechanic.. |