Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 400 g @Temperature 23.0 °C |
0.882 lb @Temperature 73.4 °F |
ASTM D1709A modified |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Dart Drop Test | 400 g @Temperature 23.0 °C |
0.882 lb @Temperature 73.4 °F |
ASTM D1709A modified |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |