Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 1.4 µm/km @Temperature 100 °C |
1.4 µm/km @Temperature 212 °F |
|
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
K Factor (ISO) | 1.4 µm/km @Temperature 100 °C |
1.4 µm/km @Temperature 212 °F |
|
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |