Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 12 µm/km @Temperature 20.0 °C |
12 µm/km @Temperature 68.0 °F |
|
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |