Mechanical Properties Metric English Comments
K Factor (ISO) 5.3 µm/km

@Temperature 100 °C
5.3 µm/km

@Temperature 212 °F
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced
Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed..
K Factor (ISO) 5.3 µm/km

@Temperature 200 °C
5.3 µm/km

@Temperature 392 °F
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..