Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.000300 GPa | 0.0435 ksi | |
Kuraray HYBRAR® Low Rebound Compound # 2 Control Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |