Polymer Property : Tensile Modulus = 0.00862 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.00862 GPa
1.25 ksi
Type IV, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W3400L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..