Mechanical Properties Metric English Comments
Tensile Modulus 0.00896 GPa
1.30 ksi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W2407L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Modulus 0.00896 GPa
1.30 ksi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable WJAX204L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Tensile Modulus 0.00896 GPa
1.30 ksi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable WJAX204V Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Modulus 0.00896 GPa
1.30 ksi
Type IV, 510 mm/min; ASTM D638
PolyOne FireCon™ CPE 1240 UV RoHS NATURAL Polyethylene, Chlorinated (CPE)
An excellent choice for low-voltage power-and-cable control cables, this RoHS compliant filled, flexible thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantages of th..
Tensile Modulus 0.00896 GPa
1.30 ksi
(0.2 in/min), Molded Properties; ASTM D638
ExxonMobil Escorene™ UL 04533EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 04533EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Fre..
Tensile Modulus 0.00896 GPa
1.30 ksi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable W2407 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne