Mechanical Properties Metric English Comments
Tensile Modulus 0.0245 GPa
3.55 ksi
Zeon Chemicals Zetpol® ZCS 2395 Hydrogenated Nitrile Elastomomer
Zeoforte® ZSC 2395 is a highly saturated copolymer of butadiene and acrylonitrile, which has been modified with the zinc salt of methacrylic acid. ZSC 2395 has excellent physical properties and a..