Polymer Property : Tensile Modulus = 0.02904 GPa
Polymer Property :
Tensile Modulus =
0.02904 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Modulus
0.02904
GPa
4.212
ksi
Network Polymers Softflex® 8103
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.