Polymer Property : Tensile Modulus = 0.0500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.000345 GPa
0.0500 ksi
ASTM D3574
Saint-Gobain Korel® K30-15 Soft Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi..
Tensile Modulus 0.000345 GPa
0.0500 ksi
ASTM D3574
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi..
Tensile Modulus 0.000345 GPa
0.0500 ksi
ASTM D3574
Saint-Gobain Korel® K40-35 Medium Deflection Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..