Polymer Property : Tensile Modulus = 0.0878 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0878 GPa

@Temperature 30.0 °C
12.7 ksi

@Temperature 86.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur..