Polymer Property : Tensile Modulus = 0.102 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.000701 GPa

@Temperature 170 °C
0.102 ksi

@Temperature 338 °F
50%RH; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 330 NC010 Nylon  (Unverified Data**)
Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers