Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in..