Polymer Property : Tensile Modulus = 0.147 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.147 GPa
21.3 ksi
TD
Kuraray HYBRAR® CF3 Mono Layer Cast Film
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Tensile Modulus 0.147 GPa
21.3 ksi
ISO 527
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane
Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr..