Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.159 GPa | 23.0 ksi | ASTM D638 |
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Tensile Modulus | 0.159 GPa | 23.0 ksi | ISO 527-2/1A/1 |
ExxonMobil LDPE LD 615BA Low Density Polyethylene Resin (European Grade) Product Description: LD 615BA is a medium flow LDPE grade, characterized by high stiffness and good toughness.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal S.. |