Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.185 GPa | 26.8 ksi | 1 mm/min |
Arkema Group Rilsan® BMV 400 TL Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,18-002,ZFlexible grade for injection molding. Available color: natural. Light and heat stabilized. Plasticizing agent free.Outstanding impact strength and tear spreading .. |
|||
Tensile Modulus | 0.185 GPa | 26.8 ksi | 1 mm/min |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |