Mechanical Properties Metric English Comments
Tensile Modulus 0.253 GPa
36.7 ksi
1 mm/min
Arkema Group Pebax® MV 1041 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 60 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....)ISO data provided ..