Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.290 GPa @Temperature 23.0 °C |
42.1 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET
(Unverified Data**) Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like .. |
|||
Tensile Modulus | 0.290 GPa | 42.1 ksi | MD; ASTM D882-A |
Borealis Borstar® FB3450 HDPE for Film Extrusion Borstar® FB3450 is a high density polyethylene. Borstar® FB3450 is well suited for multilayer coextruded films where higher stiffness and toughness than in standard LDPE and LLDPE is required. Ap.. |