Polymer Property : Tensile Modulus = 0.370 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.370 GPa
53.7 ksi
ASTM D882
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one..
Tensile Modulus 0.370 GPa
53.7 ksi
ASTM D882
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one..
Tensile Modulus 0.370 GPa
53.7 ksi
ASTM D882
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one..
Tensile Modulus 0.370 GPa
53.7 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® L 22A W 40 X PA12-I
Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st..
Tensile Modulus 0.370 GPa

@Temperature 80.0 °C
53.7 ksi

@Temperature 176 °F
ISO Data
BASF Ultramid® 8253 PA6 (Conditioned)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..
Tensile Modulus 0.370 GPa
53.7 ksi
ASTM D882
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one..