Mechanical Properties Metric English Comments
Tensile Modulus 0.379 GPa
55.0 ksi
ASTM D-882
Saint-Gobain Norton® Chemfilm® MR Fluoropolymer Cast Film
Description: Commonly used for Aerospace/Release Film ApplicationsInformation provided by Saint Gobain Performance Products.
Tensile Modulus 0.379 GPa
55.0 ksi
ASTM D-882
Saint-Gobain Norton® Chemfilm® VB Fluoropolymer Cast Film
Description: Commonly used for Aerospace/Release Film ApplicationsInformation provided by Saint Gobain Performance Products.
Tensile Modulus 0.379 GPa
55.0 ksi
ASTM D4894
Saint-Gobain Fluoroloy® A08 High Performance Seal Material
Superior heat and wear resistance; Recommended for moderate to high speed dynamic service running against soft metals; Non-abrasive Information provided by Saint-Gobain Performance Plastics.