Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.421 GPa | 61.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Tensile Modulus | 0.421 GPa | 61.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.421 GPa | 61.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.421 GPa | 61.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.421 GPa | 61.1 ksi | ISO 527 |
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |