Polymer Property : Tensile Modulus = 0.465 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.465 GPa
67.4 ksi
1 mm/min
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical..