Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 0.600 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Hyflon® PFA 120 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Tensile Modulus 0.400 - 0.600 GPa
58.0 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer
Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
MD/TD; ISO 527-3
Borealis BA11CF Polypropylene Copolymer
BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. ..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
MD/TD; ISO 527-2
Borealis BB213CF Polypropylene Copolymer
BB213CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BB213CF is recommended for food packaging..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
MD/TD; ISO 527-3
Borealis BorPure™ RD234CF Polypropylene Random Copolymer
BorPure™ RD234CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD234CF is recommended for food packaging, stationa..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
MD/TD; ISO 527-3
Borealis RD204CF Polypropylene Random Copolymer
RD204CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD204CF is recommended for blending, food packaging, high qua..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
MD/TD; ISO 527-3
Borealis RD461CF Polypropylene Random Copolymer
RD461CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD461CF is recommended for food packaging, high quality stati..
Tensile Modulus 0.500 - 0.600 GPa
72.5 - 87.0 ksi
MD/TD; ISO 527-3
Borealis RD734CF Polypropylene Random Copolymer
RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stati..
Tensile Modulus 0.500 - 0.600 GPa

@Temperature 23.0 °C
72.5 - 87.0 ksi

@Temperature 73.4 °F
1.0 mm/min; ASTM D1708
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, ..
Tensile Modulus 0.500 - 0.600 GPa

@Temperature 23.0 °C
72.5 - 87.0 ksi

@Temperature 73.4 °F
1.0 mm/min; ASTM D1708
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Tensile Modulus 0.500 - 0.600 GPa

@Temperature 23.0 °C
72.5 - 87.0 ksi

@Temperature 73.4 °F
1.0 mm/min; ASTM D1708
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Tensile Modulus 0.500 - 0.600 GPa

@Temperature 23.0 °C
72.5 - 87.0 ksi

@Temperature 73.4 °F
1.0 mm/min; ASTM D1708
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
Tensile Modulus 0.400 - 0.600 GPa

@Thickness 2.00 mm,
Temperature 23.0 °C
58.0 - 87.0 ksi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.
Copyright © lookpolymers.com All Rights Reserved